Material properties of PtIr10 and dimensions of the hydroformed micro-tubes.
Elastic modulus E | 202300 MPa |
Poisson’s ratio ν | 0.378 |
Initial yield stress σY0 | 250 MPa |
Tensile strength σUTS | 346 MPa |
Tube outer diameter d0 | 1651 μm |
Tube wall thickness t0 | 76 μm |
Tube length l0 | 8000 μm |