SEM images of fibres spun from Solution 5 with polymer/particle weight ratio 1:8. They are spun at different flowrates: (a) 0.25 mL/h, (b) 0.50 mL/h, (c) 1.00 mL/h, (d) 1.50 mL/h and (e) 2 mL/h. It is seen that higher flowrates in general promoted thicker fibres. All images are 200 um × 200 um.