Table 1
Deposition condition.
Deposition parameters | |
---|---|
Substrate | WC-6 wt.% ISO K10 Sandvik cemented carbide insert |
Filament | Tungsten wire (Ø0.25 mm) carburized |
Filament temperature Seeding Powder |
2050 ⁰C 0.50 μm Diamond Powder |
Filament to substrate distance | 10 mm |
Substrate temperature | 700 ⁰C |
Gas composition | 1% CH4 in H2 |
Chamber reaction pressure | 20 Torr |
Deposition time Water chillers Temp. |
8 hr 12 °C |